Step by Step Method for Making Graphene
This based on the paper Achieving concentrated graphene dispersions in water/acetone mixtures by the strategy of tailoring Hansen solubility parameters\r
\r
I use:\r
\r
416.75mL of acetone\r
88.25mL of deionised water\r
1.5g 325 mesh powdered flake graphite\r
\r
and that is it. You sonicate it for between 2 and 12 hours and what you get out is graphene